Coatings are often applied to structural hardware for thermal and environmental protection. In applications including aerospace propulsion, industrial processing, and power generation, components undergo rapid thermal fluctuations, which can delaminate coatings and limit their protection. This process is hard to predict, as it depends on many factors including temperature, coefficient of thermal expansion (CTE) mismatch, and coating thickness.
By assessing various thermal shock conditions, we can predict the severity of coating delamination and inform engineering design to extend coating life. Veryst used finite element analysis (FEA) to simulate flame heating of a coated metal substrate over a preexisting flaw. As shown in Figure 1, the flame causes local thermal expansion and drives buckling delamination.

The model predicts that lower flame temperatures reduce the extent of delamination, as shown in Figure 2. In these simulations, the coating surface is locally exposed to a flame for 1 second, and then the flame is removed. At a flame temperature of 2100 K, the delamination front grows 5.4 mm radially. Lower flame temperatures cause less delamination front growth, with 1300 K approaching zero delamination.

The model also demonstrates the effects of coating thickness on delamination, as shown in Figure 3. Over the range of coating thicknesses shown with a flame temperature of 1900 K, delamination peaks at a coating thickness of 150 µm. This peak is the result of competing effects:

Veryst successfully modeled the complex process of coating delamination due to thermal shock using high-fidelity finite element analysis (FEA) across a range of flame temperatures and coating thicknesses. Our model enables engineers to predict the extent of coating delamination under various operating conditions and material combinations, which can reduce the amount of testing needed and supports coating durability.