UT006

Tensile creep testing (up to 12 hours)

Description
A uniaxial tensile specimen is loaded to a specified stress level.  The imposed stress is maintained for up to 12 hours and the stress/strain response of the material is measured.  The specimen is unloaded to zero stress at the end of the specified time duration.  Strain is measured using Digital Image Correlation (DIC) or a clip-on extensometer.

Example Data

UT006 Fig.1 Plot
UT006 Fig.2 Plot


Temperature Options
This test can generally be performed at any temperature between -80ºC and 280ºC.

  • CT: Cryogenic temperatures (-80ºC to 20ºC)
  • RT: Room temperature (~ 20ºC)
  • HT: High temperatures (20ºC to 280ºC)


Note: The use of the temperature chamber for high and low temperature tests limits the crosshead displacement for these tests.  Some combinations of material, temperature, and specimen geometries may not be possible to complete to failure.

Strain Rates
Strain rates up to ~ 1/s are possible, depending on specimen geometry.

Applicable Standards
ASTM D638, ISO 527

Data Provided
Time, Engineering Strain, Engineering Stress

Specimen Requirements
ASTM D638 or ISO 527 "dog-bone" geometries are preferred.  Comparable non-standard dog-bone or cylindrical geometries are also possible.

Note that we request extra specimens to ensure a sufficient supply of specimens for valid testing.

Veryst can also assist in molding standard and non-standard test specimens.  Please contact us if you are interested in discussing this option.

Replicates Recommended
One - three (1-3)

More Information